LOW SHRINK, HIGH CONVERSION


EXOTHANE Elastomers

Do not sacrifice conversion and the risk of residual monomer contamination to achieve low-shrink properties.  New testing has demonstrated that EXOTHANE(TM) Elastomers have low shrinkage stress, low volumetric shrinkage, AND high conversion.

  • Exothane 8, 94% Conversion, 3% Shrinkage, high % elongation
  • Exothane 26, 96% Conversion, 4% Shrinkage, increased flexibility/toughness
  • Exothane 32, 97% Conversion, 3% Shrinkage, low color and low viscosity

This new data, in addition to superior toughness, tensilse strength and percent elongation make the EXOTHANE product line ideal form many applications including, low-shrink dental restoratives, non-curling industrial coatings, unique UV nail enhancements, tougher anaerobic adhesives and more.